Hi all,

Which parts are phosphate and oil finish on a Holley 715/  I've got a non-66 version and want to make it more correct.  Thanks!


Jbarela


Bob Gaines

Quote from: gimmea250swb on November 03, 2019, 08:24:29 PM
Hi all,

Which parts are phosphate and oil finish on a Holley 715/  I've got a non-66 version and want to make it more correct.  Thanks!
Accelerator pump arm and the C clip are typically forgotten about.
Bob Gaines,Shelby Enthusiast, Shelby Collector , Shelby Concours judge SAAC,MCA,Mid America Shelby

gt350hr

  Choke rod and secondary return linkage too. Black oxide is what Holley used. make sure the pump lever is the correct early version. Plating a later version will stick out like a sore thumb. Be sure and not plate the screw , spring and contact pad , they were cad/dull zinc. Restorers tend to use too much gold irridte .